1.  Zeller-Plumhoff B., Gile M., Priebe M., Słomińska H., Boll B., Wiese B., Würger T., Willumeit-Römer R., Horst Meißner R., Exploring key ionic interactions for magnesium degradation in simulated body fluid – a data-driven approach, Corrosion Science, ISSN: 0010-938X, DOI: 10.1016/j.corsci.2021.109272, Vol.182, pp.1-109272-13, 2021

Abstract:
We have studied the degradation of pure magnesium wire in simulated body fluid and its subsets under physiological conditions to enable the prediction of the degradation rate based on the medium's ionic composition. To this end, micro-computed tomography and scanning electron microscopy with energy-dispersive X-ray spectroscopy were used, followed by a tree regression analysis. A non-linear relationship was found between degradation rate and the precipitation of calcium salts. The mean absolute error for predicting the degradation rate was 1.35 mm/yr. This comparatively high value indicates that ionic interactions were exceedingly complex or that an unknown parameter determining the degradation may exist.

Keywords:
magnesium degradation, simulated body fluid, MicroCT, tree regression

Affiliations:
Zeller-Plumhoff B. - other affiliation
Gile M. - other affiliation
Priebe M. - other affiliation
Słomińska H. - IPPT PAN
Boll B. - other affiliation
Wiese B. - other affiliation
Würger T. - other affiliation
Willumeit-Römer R. - other affiliation
Horst Meißner R. - other affiliation
2.  Meyer S., Wolf A., Sanders D., Iskhakova K., Ćwieka H., Bruns S., Flenner S., Greving I., Hagemann J., Willumeit-Römer R., Wiese B., Zeller-Plumhoff B., Degradation analysis of thin Mg-xAg wires using X-ray near-field holotomography, Metals, ISSN: 2075-4701, DOI: 10.3390/met11091422, Vol.11, No.9, pp.1422-1-12, 2021

Abstract:
Magnesium–silver alloys are of high interest for the use as temporary bone implants due to their antibacterial properties in addition to biocompatibility and biodegradability. Thin wires in particular can be used for scaffolding, but the determination of their degradation rate and homogeneity using traditional methods is difficult. Therefore, we have employed 3D imaging using X-ray near-field holotomography with sub-micrometer resolution to study the degradation of thin (250 μm diameter) Mg-2Ag and Mg-6Ag wires. The wires were studied in two states, recrystallized and solution annealed to assess the influence of Ag content and precipitates on the degradation. Imaging was employed after degradation in Dulbecco’s modified Eagle’s medium and 10% fetal bovine serum after 1 to 7 days. At 3 days of immersion the degradation rates of both alloys in both states were similar, but at 7 days higher silver content and solution annealing lead to decreased degradation rates. The opposite was observed for the pitting factor. Overall, the standard deviation of the determined parameters was high, owing to the relatively small field of view during imaging and high degradation inhomogeneity of the samples. Nevertheless, Mg-6Ag in the solution annealed state emerges as a potential material for thin wire manufacturing for implants.

Keywords:
X-ray computed tomography, magnesium-silver alloy, wire, degradation, near-field holotomography

Affiliations:
Meyer S. - other affiliation
Wolf A. - other affiliation
Sanders D. - other affiliation
Iskhakova K. - other affiliation
Ćwieka H. - IPPT PAN
Bruns S. - other affiliation
Flenner S. - other affiliation
Greving I. - other affiliation
Hagemann J. - other affiliation
Willumeit-Römer R. - other affiliation
Wiese B. - other affiliation
Zeller-Plumhoff B. - other affiliation

Category A Plus

IPPT PAN

logo ippt            Pawińskiego 5B, 02-106 Warsaw
  +48 22 826 12 81 (central)
  +48 22 826 98 15
 

Find Us

mapka
© Institute of Fundamental Technological Research Polish Academy of Sciences 2024